Plasma Spray Coatings for Superalloys

Plasma Spray Coatings for Superalloys

AngličtinaMäkká väzbaTlač na objednávku
Singh, Harpreet
VDM Verlag Dr. Müller
EAN: 9783639132540
Tlač na objednávku
Predpokladané dodanie v piatok, 13. decembra 2024
83,35 €
Bežná cena: 92,61 €
Zľava 10 %
ks
Chcete tento titul ešte dnes?
kníhkupectvo Megabooks Banská Bystrica
nie je dostupné
kníhkupectvo Megabooks Bratislava
nie je dostupné
kníhkupectvo Megabooks Košice
nie je dostupné

Podrobné informácie

Superalloys are well known materials for
high temperature applications. Although the
superalloys have adequate mechanical strength at
elevated temperatures, yet they often lack resistance
to oxidizing/corroding environments during long time
exposures. One possible way to combat the problem
constitutes the use of protective coatings on the
superalloys. Among the various techniques used for
deposition of coatings, plasma spraying is a
versatile technology that has been successful as a
reliable cost-effective solution for many industrial
problems.In the present book, high temperature
oxidation behavior of some Ni- and Fe- based
superalloys has been explained with and without the
application of plasma sprayed coatings in air, as
well as, in a simulated boiler (Na2SO4-60%V2O5)
environment.Characterization and high temperature
oxidation behavior of four coatings; Ni-22Cr-10Al-1Y
(NiCrAlY), Ni-20Cr, Ni3Al and Stellite-6 has been
elaborated with the help of Optical microscopy,
Scanning Electron Microscopy/Energy Dispersive
Spectroscopy and Electron Probe Micro Analysis.The
effectiveness of the coatings has been discussed on
the basis of weight change data.